Preparation of Mica Nacreous Pigment by Urea Neutralization Method
LI Zhen-rong,SHAO Jun-jie,LI Guang-fu(College of Light Industry,Liaoning University,Shenyang 110036,China)
(College of Light Industry,Liaoning University,Shenyang 110036,China

Abstract
Reference
Related Articles
Download: PDF (191KB)   HTML 1KB   Export: BibTeX or EndNote (RIS)      Supporting Info
Abstract The preparation of mica nacreous pigment by urea neutralization method was discussed.SEM and whiteness meter were used to determine the optimum condition.80% of the urea is added one-time into the mica suspension and the other 20% into the titanium salt.The better hydrolyzing temperature is 90 ��.The volume of 10% titanium solution is 28 mL corresponding to 10 g mica.Titanium solution is dropped into the mica suspension with speed of 28 mL /h.The mass ratio of urea to titanium is 3�� 1.The optimum stirring speed is 200 r /min.The optimum calcination condition is 950 �� for 1 hour.
Service
Email this article
Add to my bookshelf
Add to citation manager
Email Alert
RSS
Articles by authors
Keywords��   
Received 2010-07-15; published 2010-07-15
Cite this article:   
LI Zhen-rong,SHAO Jun-jie,LI Guang-fu.Preparation of Mica Nacreous Pigment by Urea Neutralization Method[J]  Chemcial Industry and Engineering, 2010,V27(4): 334-339
Copyright 2010 by Chemcial Industry and Engineering