Abstract��
For lowering the B_2O_3 and CaO content in magnesia from brine by two-step-overlimed method,a modification was proposed,i.e.,the brine deboronized by resin instead of raw-brine is used in the secend step.By this modification the B_2O_3 content in magnesia is 63% lower than that by conventional two-step method.